Components | two |
Weight mixing ratio | 100/35 |
Viscosity/two5 ° C, cp | two00-500 |
Operating time two5 ° C (100g) hours | >8 |
Recommended curing conditions | 3hrs@80 °C 24-48hrs@25 °C |
appearance | transparent |
proportion | one point one |
Hardness, Shore | D-eighty-two |
Refractive index | one point five three |
Shear strength, psi | two thousand and three hundred |
Glass transition temperature (Tg) ° C | eighty-two |
Linear expansion coefficient (10 ⁻⁶/° C) | sixty-one |
working temperature | -55°C to 200°C |
Thermal conductivity (W/mK) | NA |
Volume resistance (ohm cm) | 1×10fourteen |