Components | two |
Weight mixing ratio | 100/50 |
Viscosity/two5 ° C, cp | 4000-7000 |
Operating time two5 ° C (100g) | 30min |
Recommended curing conditions | 3hrs@65 °C two4-48hrs@25 °C |
appearance | transparent |
proportion | one point one |
Hardness, Shore | D-86 |
Refractive index | one point five four |
Shear strength, psi | three thousand and one hundred |
Glass transition temperature (Tg) ° C | seventy-two |
Linear expansion coefficient (10 ⁻⁶/° C) | sixty-two |
working temperature | -55°C to125°C |
Thermal conductivity (W/mK) | NA |
Volume resistance (ohm cm) | 1×10thirteen |