| Components | two |
| Weight mixing ratio | 100/two5 |
| Viscosity/two5 ° C, cp | 500-eighty0 |
| Operating time two5 ° C (100g) | 30-40min |
| Recommended curing conditions | 3hrs@65 °C 24-48hrs@25 °C |
| appearance | transparent |
| proportion | one point one six |
| Hardness, Shore | D-85 |
| Refractive index | one point five two |
| Shear strength, psi | three thousand |
| Glass transition temperature (Tg) ° C | eighty |
| Linear expansion coefficient (10 ⁻⁶/° C) | fifty-nine |
| working temperature | -55°C to200°C |
| Thermal conductivity (W/mK) | NA |
| Volume resistance (ohm cm) | 8×10fourteen |