Components | two |
Weight mixing ratio | 100/10 |
Viscosity/two5 ° C, cp | 1000 - 1500 |
Operating time two5 ° C (100g) hours | 3-4 |
Recommended curing conditions | 1hrs@100 °C 8hrs@80 °C |
appearance | silvery |
proportion | two point seven |
Hardness, Shore | D-75 |
Shear strength, psi | one thousand and one hundred |
Glass transition temperature (Tg) ° C | sixty-four |
Linear expansion coefficient (10 ⁻⁶/° C) | sixty-two |
working temperature | -50°C to 155°C |
Thermal conductivity (W/mK) | one point six |
Volume resistance (ohm cm) | zero point zero zero zero six |