Components | two |
Mixing ratio | 100/100 |
Viscosity/two5 ℃, cps | five hundred thousand |
Operating time two5 ℃ (100g) | 45min |
Recommended curing conditions | two4hrs@25 ℃+ 1hrs@100 ℃ 2hrs@80 ℃ |
appearance | black |
Specific gravity, g/cm³ | two point one |
Hardness, Shore | D-81 |
Shear strength, psi | three thousand |
Glass transition temperature (Tg) ℃ | ninety |
Linear expansion coefficient (10 ⁻⁶/℃) | seventy-seven |
working temperature | -55℃ to 200℃ |
Thermal conductivity (W/mK) | one point three five |
Volume resistance (ohm cm) | 3×10fourteen |