Components | two |
Mixing ratio | 100/100 |
Viscosity/two5 ℃, cps | >100000 |
Operating time two5 ℃ (100g) | 90-1two0min |
Recommended curing conditions | 3hrs@65 ℃ 24-48hrs@25 ℃ |
appearance | grey |
Specific gravity, g/cm³ | one point seven |
Hardness, Shore | D-86 |
Shear strength, psi | two thousand and eight hundred |
Glass transition temperature (Tg) ℃ | eighty |
Linear expansion coefficient (10 ⁻⁶/℃) | sixty |
working temperature | -55℃ to 1sixty℃ |
Thermal conductivity (W/mK) | two point seven |
Volume resistance (ohm cm) | 3×10fourteen |