Home——Products——Single component epoxy structural adhesive
EB-350-4T-FL

EB-350-4T-FL

Componentsonechemical compositionepoxy resinViscosity/25 ℃, cps>eight hundred thousandOperating time 80 ℃ (one00g)20minRecommended curing conditionsonehrs@one00 ℃ + 1hrs@150 ℃2hrs@125 ℃30min@150 ℃20min@175 ℃appearanceblackSpecific gravity, g/cm³one point five sixHardness
EB-350-4T

EB-350-4T

Componentsonechemical compositionepoxy resinViscosity/25 ℃, cps>eight hundred thousandOperating time 25 ℃ (one00g)3monthRecommended curing conditionsonehrs@one00 ℃ + 1hrs@150 ℃2hrs@125 ℃30min@150 ℃20min@175 ℃appearanceblackSpecific gravity, g/cm³one point fiveHardness, S
EB-403-1LV-T1

EB-403-1LV-T1

Componentsonechemical compositionepoxy resinViscosity/25 ℃, cps800000-one200000Operating time 25 ℃ (one00g)4monthRecommended curing conditionsonehrs@100 ℃ + 1hrs@fifteen0 ℃30min@fifteen0 ℃appearanceblackSpecific gravity, g/cm³two point twoHardness, ShoreD-90Shear strength, psitwo thousan
EB-403-1LV

EB-403-1LV

Componentsonechemical compositionepoxy resinViscosity/25 ℃, cpsfifteen0000-250000Operating time 25 ℃ (one00g)3monthRecommended curing conditionsonehrs@one00 ℃ + 1hrs@fifteen0 ℃30min@fifteen0 ℃appearanceblackSpecific gravity, g/cm³two point oneHardness, ShoreD - 90Shear strength, psitwo t
EB-350-1LE

EB-350-1LE

Component 1 Chemical composition Epoxy resin viscosity/25 ℃, cps40000-60000 Storage conditions 25 ℃ 4month Recommended curing conditions 2hrs@125 ℃ 30min@150 ℃ Appearance Black specific gravity, g/cm ³ 1.6 hardness, ShoreD-91 shear strength, psi2400 Glass transition temperature (Tg) ℃ 120 Linear expansion coefficient (10 ⁻⁶/℃) 28 Working temperature -55 ℃ to 175 ℃ Thermal conductivity (W/mK) 0.5 Volume resistance (ohm cm) 1x1015
EB-350-3LV

EB-350-3LV

Component 1 Chemical composition Epoxy resin viscosity/25 ℃, cps55000-65000 Storage conditions 25 ℃ 3month Recommended curing conditions 1hrs@100 ℃+ 1hrs@150 ℃ 1hrs@125 ℃ 20min@150 Appearance black specific gravity, g/cm ³ 1.56 hardness, ShoreD-91 shear strength, psi3500 glass transition temperature (Tg) ℃ 130 linear expansion coefficient (10 ⁻⁶/℃) 45 working temperature -55 ℃ to 220 ℃ thermal conductivity (W/mK) 0.4 volume resistance (ohm cm) 6x1015
EB-350-1LV-M2

EB-350-1LV-M2

Componentsonechemical compositionepoxy resinViscosity/25 ℃, cpsfifteen000-30000Storage conditions: 25 ℃3monthRecommended curing conditionsonehrs@one00 ℃+ onehrs@fifteen0 ℃2hrs@125 ℃30min@fifteen0 ℃20min@175 ℃appearanceblackSpecific gravity, g/cm³one point fiveHardness, ShoreD-91Shear strengt
EB-350-4LV

EB-350-4LV

Componentsonechemical compositionepoxy resinViscosity/25 ℃, cps200000-300000Storage conditions: 25 ℃4monthRecommended curing conditionsonehrs@one00 ℃+ onehrs@fifteen0 ℃2hrs@125 ℃30min@fifteen0 ℃20min@175 ℃appearanceblackSpecific gravity, g/cm³one point fiveHardness, ShoreD-91Shear strength,